What 30-minus actually means
"30-minus" is shorthand for crumb rubber that passes a No. 30 U.S. standard sieve, which has a 600-micron (0.6 mm, about 0.024 in) opening. Everything in the sack is that size or smaller, down into the fines. It is not a single particle size. It is a distribution, and the shape of that distribution is what decides whether it works in your process.
Under ASTM D5603, a product designated 30 mesh has zero retained on the No. 20 "zero screen" (850 µm) and no more than 10% retained on the No. 30 designation screen. Particle size distribution is measured with the vibratory sieve-shaker method in ASTM D5644. When we say a lot is 30-minus, we can send the sieve numbers behind it.
Our typical production curve for 30-minus looks like this (representative, not a lot guarantee):
| Sieve | Opening | Typical % retained |
|---|---|---|
| No. 30 | 600 µm | ~12% |
| No. 35 | 500 µm | ~23% |
| No. 40 | 425 µm | ~18% |
| No. 50 | 300 µm | ~22% |
| No. 80 | 180 µm | ~17% |
| No. 100 | 150 µm | ~4% |
That spread, with a real chunk of material in the 40-to-80 range, is why 30-minus is the workhorse fine grind in this industry.
Why buyers pick 30-minus
- Volume you can actually get. We are holding millions of pounds. No allocation games, no "we'll have some next quarter."
- The asphalt sweet spot. FHWA's 2020 report on recycled tire rubber in asphalt (FHWA-HIF-20-043) notes that 600-420 µm (30 to 40 mesh) particles are the most typical size for terminal-blend rubber-modified binders, which the industry "commonly referred to as '30 minus rubber.'" The same report puts today's dry-process GTR in the 30-to-40 mesh range.
- Fine enough to disappear into a compound. Molders blending crumb into a bound product, and formulators adding filler to sealants, get a smoother surface than with coarse crumb.
- Easy to ship. It flows, it bags tight, and it stacks in a dry van without drama.

Where 30-minus goes
Rubber-modified asphalt
Terminal-blend binders (RMB) typically blend 5 to 15 percent GTR by weight of binder, using 30-80 mesh rubber, with 30-40 mesh most common (FHWA-HIF-20-043). Dry-process mixes add roughly 10 percent GTR by weight of binder, which FHWA works out to about 0.5 percent of the mix, or about 10 pounds of rubber per ton of asphalt mixture. See our rubberized asphalt page for the full breakdown.
Molded and bonded products
Fine crumb gives molded goods a tighter, smoother face. Many molders run 30-minus as a surface layer over a coarser 10-20 mesh core.
Sealants, coatings and compounding
Some formulators want 30-minus; others need 40 mesh or 80 mesh powder. Send your target curve and we'll tell you which fits.
Export and distribution
30-minus is a common export grade because the specification is well understood worldwide. See export.
Worked examples
Example 1: A dry-process paving job
A contractor is placing 20,000 tons of dry-process rubber-modified mix. Using FHWA's rule of thumb of about 10 lb of GTR per ton of mixture:
- 20,000 tons × 10 lb/ton = 200,000 lb of 30-minus
- At a typical ~2,000 lb per supersack, that's about 100 supersacks
- At a typical 40,000-44,000 lb per 53-ft dry van, that's about 5 truckloads
Your mix design and agency spec set the real dosage. The math just tells you whether a supplier can cover the job. We can, out of stock.
Example 2: A terminal blender's monthly program
A terminal producing 1,000 tons of rubber-modified binder a month at 10% GTR by weight of binder needs:
- 1,000 tons × 10% = 100 tons = 200,000 lb of 30-minus per month
- That's about 5 loads a month, roughly one a week
That is exactly the kind of recurring program we want to quote.
Need 30-minus by the truckload? Send grade, volume, delivery city/ZIP and your target price.
Request a QuoteSpec sheet
| Nominal size | 30 mesh and finer (30-minus) |
|---|---|
| Full sieve distribution | Typical production (representative): No.30 ~11.8% retained / ~88% passing; No.35 ~23%; No.40 ~18%; No.50 ~22%; No.80 ~17%; No.100 ~4%. Full lot sieve on request. |
| Sieve standard / test method | ASTM D5644 (lot sieve report on request) |
| Residual steel (max) | Production target <0.01% by weight (lot COA) |
| Fiber (max) | Production target ≤0.01% by weight (ASTM D5603) |
| Moisture (max) | typical ≤1.0% by weight (ASTM D5603) |
| Specific gravity | typical ~1.15 |
| Source / classification | typical recycled passenger and/or truck tires · ground rubber (ASTM D5603) |
| Availability | Large-volume inventory in stock — allocation confirmed at quote |
| Packaging | Supersacks / bulk bags, with or without pallets · typical ~2,000 lb net per sack (confirmed on quote). Gaylords or loose bulk on request. |
| Minimum order | typical one supersack (~2,000 lb) · truckload programs preferred |
| Lead time | typical 3–10 business days for in-stock grades; allocation confirmed at quote |
typical = representative or industry-standard value, confirmed per lot and in your written quote. Mesh labels alone don't describe the full distribution.
Download the 30-minus PDF data sheet. Values marked typical are representative; every quote is backed by lot data on request.
Packaging and loading
- Supersacks (bulk bags), with or without pallets. Typical net weight around 2,000 lb per sack, confirmed on your quote.
- Truckloads: typically 40,000-44,000 lb per 53-ft dry van, depending on sack count and pallets.
- FOB Central Ohio or delivered. Tell us your city, state and ZIP and we'll price freight.
More detail in our supersack shipping and freight guide.
Frequently asked questions
Is 30-minus the same as 30 mesh?
In everyday trade talk, yes. Technically, ASTM D5603 defines a 30-mesh product as zero retained on the No. 20 sieve and no more than 10% retained on the No. 30 sieve. Ask for the lot's sieve report so you're comparing real numbers, not labels.
How much 30-minus do you have?
Millions of pounds in stock as of this writing, packed in supersacks in Central Ohio. Allocation is confirmed in writing on your quote.
Will your 30-minus meet my DOT spec?
Many DOT specs call out gradation, fiber, metal, moisture and sometimes source requirements. Send the spec section and we'll check the lot against it before you buy. We don't claim compliance with any agency spec until it's documented for your lot.
Can I get a sample?
Yes. Note it on the quote form. A 1-2 kg lab sample is typical; freight is confirmed separately.
What's the minimum order?
Typically one supersack, but truckload and recurring programs get our best attention and best pricing.
Do you publish prices?
No. Price depends on volume, packaging and freight to your ZIP. Tell us what you pay now or what you want to pay, and we'll give you a straight yes or no.
Sources: ASTM D5603-23 and D5644-23 (astm.org); FHWA, Resource Responsible Use of Recycled Tire Rubber in Asphalt Pavements, FHWA-HIF-20-043, 2020 (PDF).